INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Need help cutting crs 0.040 with shop air

Need help cutting crs 0.040 with shop air

Need help cutting crs 0.040 with shop air

(OP)
Hi the machine is Amada Fo3015NT. we are not able to get a nice cut. Someone have cutting condition for this type of material?

RE: Need help cutting crs 0.040 with shop air

try using the cut condition for stainless steel of the same thickness, but change your assist gas to shop air.

RE: Need help cutting crs 0.040 with shop air

(OP)
Thanks for your reply. I think we don't have a good air, cause we still have a lot of dross. not able to get a clean cut.

RE: Need help cutting crs 0.040 with shop air

if you can post a picture of the parts edge and of the cut condition screen, there are a few really good experts here who can help a lot if you provide enough information. I am not an expert, but things i would try is lowering air pressure, going up and down with focus, increasing and decreasing feedrate.

"I am stuck on Band-Aid brand, 'cause they are stuck on me"

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources