Where can I find physical/mechanical properties of ASTM A36 carbon steel and 304 Stainless at temperatures from around 500 deg F to 700 deg F?





RE: Properties of A36 Steel & 304 SS @ Elevated Temperatures (500-700 deg F)
MMPDS-05 pages 2.257-2.259
RE: Properties of A36 Steel & 304 SS @ Elevated Temperatures (500-700 deg F)