Records of VT acc. to B31.3
Records of VT acc. to B31.3
(OP)
Hi there,
B31.3 (para. 344.2.2) says that records of individual visual examinations are not required , except for those of in-process examination as specified in para. 344.7. So i have to record all points in 344.7 any time? For example the condition of the weld between every pass?
By whom? VT personnel?
Greets
B31.3 (para. 344.2.2) says that records of individual visual examinations are not required , except for those of in-process examination as specified in para. 344.7. So i have to record all points in 344.7 any time? For example the condition of the weld between every pass?
By whom? VT personnel?
Greets





RE: Records of VT acc. to B31.3
RE: Records of VT acc. to B31.3
RE: Records of VT acc. to B31.3
RE: Records of VT acc. to B31.3
And what do i have to record when just VT is required and no RT and PT will be done? The requirements of Section V T-990?
RE: Records of VT acc. to B31.3
RE: Records of VT acc. to B31.3