INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Concrete Testing Tools

Concrete Testing Tools

Concrete Testing Tools

(OP)
Has anyone ever heard of or tried Giatec's XCell product or any other products? The company specializes in concrete durability testing. Debating on whether or not their company has the right equipment for my firm.

Does anyone have any information on other firms who may carry similar and better products?

Website: http://www.giatecscientific.com/

RE: Concrete Testing Tools

Looks like a fancy wireless/Bluetooth compatible half-cell potential test unit for RC concrete corrosion testing.

Never used that brand before.

If you want to determine (test for) half-cell corrosion potentials then it may be worth considering. My guess is it will be expensive, but other competing equipment is typically more than $5k, depending if you go with probe or wheel-based electrodes.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources