CO2 Corrosion resistant material
CO2 Corrosion resistant material
(OP)
Dear all,
My case is as follow:
The Gas composition include 90.5% Methane and 0,93% of CO2. The temperature is about 25DegC. Condensate production will be 1000bbl/d. The water amount, will be about 1000 bbl/d, after first 2 year of production.
Do I need to consider the concentration of CO2 (and water) as a problem? Do I need to use special corrosion resistant material for pressure vessels or can be SA516? Is this concentration - 0,93% of CO2 can be considered as dangerous for my case.
Best regards
My case is as follow:
The Gas composition include 90.5% Methane and 0,93% of CO2. The temperature is about 25DegC. Condensate production will be 1000bbl/d. The water amount, will be about 1000 bbl/d, after first 2 year of production.
Do I need to consider the concentration of CO2 (and water) as a problem? Do I need to use special corrosion resistant material for pressure vessels or can be SA516? Is this concentration - 0,93% of CO2 can be considered as dangerous for my case.
Best regards





RE: CO2 Corrosion resistant material
Steve Jones
Corrosion Management Consultant
http://www.linkedin.com/pub/8/83b/b04
All answers are personal opinions only and are in no way connected with any employer.