INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

API 2h gr50 to 316 ss

API 2h gr50 to 316 ss

API 2h gr50 to 316 ss

(OP)
Hey guys I'm looking for some guidance on running a welding procedure on api 2h gr50 to 316ss and it requires charpy it is to AWS d1.1. Or should I be looking in AWS d1.6? Help please.

Thanks in advance
Qcpeewee

RE: API 2h gr50 to 316 ss

Sorry to be brusque but you need to contact a local welding engineer.

"If you don't have time to do the job right the first time, when are you going to find time to repair it?"

RE: API 2h gr50 to 316 ss

Read the preface to AWS D1.1 - it is only valid for mild carbon steel, with thicknesses above that of sheetmetal. Thus it is impossible to use D1.1.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources