AWS D1.5 CVN testing
AWS D1.5 CVN testing
(OP)
Hello,
I have a question concerning cvn testing to AWS D1.5. When calculating the average ft/lb for the 5 weld metal cvn samples are the high/low values excluded or are all five specimens averaged?
Thank you.
I have a question concerning cvn testing to AWS D1.5. When calculating the average ft/lb for the 5 weld metal cvn samples are the high/low values excluded or are all five specimens averaged?
Thank you.





RE: AWS D1.5 CVN testing