A707L3CL3F65 CE=.40
A707L3CL3F65 CE=.40
(OP)
I am looking for someone with expierence in testing A707 L3CL3 WITH A LOW CE=.40 AND WHAT MECHANICAL PROPERIES WERE obtained the market of pipeline flanges in south america is coming out with specs of ce=.40 MAX THIS SHOULD MAKE MECHANICALS PROPERTIES VERY POOR AND I AM TRYING TO GET SOME INSIGHT AT WHAT I MAY DISCOVER THANKS






RE: A707L3CL3F65 CE=.40