I have modeled compression test on concrete cube in Abaqus/Explicit. For concrete I have used Concrete damaged plasticity model. I have assigned displacement as BC (Smooth amplitude) in Reference Point at the top of the cube, and I have coupled RP with the top of the cube. For concrete cube I have used C3D8R elements.
For history output I have requested Reaction force in RP and energies for whole model.
But job won't finish. I get an error:
The part map file "D:\Marko\Concrete\Compression.prt" is corrupt, does not exist, or cannot be opened.
The elements contained in element set ErrElemExcessDistortion-Step1 have distorted excessively.
I am sending you pictures of Reaction Force and PE and PEEQ of Cube (results until job cancelation).
Can anyone tell me why and give me some suggestions?
I have modeled compression test on concrete cube in Abaqus/Explicit. For concrete I have used Concrete damaged plasticity model. I have assigned displacement as BC (Smooth amplitude) in Reference Point at the top of the cube, and I have coupled RP with the top of the cube. For concrete cube I have used C3D8R elements.
For history output I have requested Reaction force in RP and energies for whole model.
But job won't finish. I get an error:
The part map file "D:\Marko\Concrete\Compression.prt" is corrupt, does not exist, or cannot be opened.
The elements contained in element set ErrElemExcessDistortion-Step1 have distorted excessively.
I am sending you pictures of Reaction Force and PE and PEEQ of Cube (results until job cancelation).
Can anyone tell me why and give me some suggestions?