INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

SS vs SST

SS vs SST

SS vs SST

(OP)
Could some one give me an insight as to what is the difference between "SS & SST" in terms of stainless steel material ie 416 SS & 416 SST.

My first instinct was that they were the same both SS and SST stands for stainless steel, just written in a fancy manner.

I may be wrong. If you feel so it would be great to know.

Thank you for your time.

veneeth george
piping engineer - offshore rigs

RE: SS vs SST

They are one in the same abbreviation. It should be listed as Type 416 with no suffix.

RE: SS vs SST

(OP)
metlonis - that post was an interesting read.
metengr - that make sense

Thank you for your time.

RE: SS vs SST

My response would be AO.

Which stands for Acronym Overload.

"If you don't have time to do the job right the first time, when are you going to find time to repair it?"

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources