INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

concrete curing CSA 23.1 table 20 clarification?

concrete curing CSA 23.1 table 20 clarification?

concrete curing CSA 23.1 table 20 clarification?

(OP)
Any Canadians can clarify something from CSA code? A23.1 looking at table 20 for concrete curing. My question is, what is meant by 10'C? Is it the ambient temperature, concrete temperature, surface temperature, or what?

"1 Basic curing 3 d at  10 °C or for the time necessary to attain 40% of the specified strength."

Thanks
Cam

RE: concrete curing CSA 23.1 table 20 clarification?

basically it means cure at above freezing. 10c equal 50 f, most spec calls for curing at 72f, but your spec sounds like field cure above 50f

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources