We are going to manufacture Wellhead equipment with cladded internals(API 6A/Base metal AISI 4130 + Inco 625 cladding).
As per API 6A, hardness testing on cladded surface is required for welding procedure qualification only whereas client is instructing us to carry it on production part cladded surface.
My question is “Does hardness testing is mandatory for cladding after production as per API 6A ?”.