API 650 STD STAMP has fallen off my oil storage tank!
API 650 STD STAMP has fallen off my oil storage tank!
(OP)
Gentlemen,
In the near future I will have to hire a contractor to make some welding repairs on some small pits on top of my oil storage tank. It originally had an API 650 STD stamp on the tank but has fallen off in the past. So the tank doesn't have any stamp indication of an API STF on it currently. Since the contractor will be following all of the API 650/653 guidelines to repair the small pitting damage, what stamp should be go back on the tank? Should it be a API STD 653 stamp since it is a "repair" to an original tank? What is the best way to recertify this tank and which API standard to use?
In the near future I will have to hire a contractor to make some welding repairs on some small pits on top of my oil storage tank. It originally had an API 650 STD stamp on the tank but has fallen off in the past. So the tank doesn't have any stamp indication of an API STF on it currently. Since the contractor will be following all of the API 650/653 guidelines to repair the small pitting damage, what stamp should be go back on the tank? Should it be a API STD 653 stamp since it is a "repair" to an original tank? What is the best way to recertify this tank and which API standard to use?





RE: API 650 STD STAMP has fallen off my oil storage tank!
Generally, if a nameplate has been lost and it can be positively identified what the tank is and other pertinent information, the nameplate can be replaced. If it's the "mystery tank" that nobody knows anything about who built it or when or how, then that's not an option.
API-653 nameplates are mandated for reconstructed tanks, but it is really meaningless to put an API-653 nameplate on a tank due to minor repairs being done. That is, somebody can certify that certain repairs were performed to API-653, but that doesn't mean the tank met API-650 in the first place.
RE: API 650 STD STAMP has fallen off my oil storage tank!
RE: API 650 STD STAMP has fallen off my oil storage tank!
RE: API 650 STD STAMP has fallen off my oil storage tank!