Can someone a price comparison for materials like below?
WCB, CF8M, Alloy 20, 904L, Inconel 625, Hastelloy C276, etc.
Like 1: 2 : 2.5 : 2.5 : 6 : 7 etc
WCB, CF8M, Alloy 20, 904L, Inconel 625, Hastelloy C276, etc.
Like 1: 2 : 2.5 : 2.5 : 6 : 7 etc





RE: Price Levels
In general 625 and C276 have very similar prices, about 8-9x the 304 price.
Alloy 20 and 904L are used very little, so they are more expensive than the alloy content would indicate.
At todays Ni and Mo prices 316 is about 1.4x the 304 price (hence the move to lean duplex grades in place of 316).
= = = = = = = = = = = = = = = = = = = =
Plymouth Tube