INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Effect of methanol in co2 corrosion

Effect of methanol in co2 corrosion

Effect of methanol in co2 corrosion

(OP)
Dear All,
We are using methanol injection to avoid hydrate formation in sweet service. Is this effect on Co2 corrosion? CO2 corrosion rate is decreasing by adding glycol concentration. I want to know the effect of methanol in co2 corrosion?
Please clarify.

Thanks

RE: Effect of methanol in co2 corrosion

It is not the methanol, but the oxygen you can introduce with the methanol. You can get inhibited methanol, most chemical suppliers will already sell it this way.

RE: Effect of methanol in co2 corrosion

The methanol absorbs the water so there is no aqueous electrolyte.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources