INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

PWHT CODE REQUIREMENTS

PWHT CODE REQUIREMENTS

PWHT CODE REQUIREMENTS

(OP)
dear members

To release internal stress we will perform PWHT. In how many cases ASME CODE is recommending PWHT like Thickness, P.NO . I would like to know what are the code recommended cases for PWHT.

Vijaykumar eatukuri

RE: PWHT CODE REQUIREMENTS

Please review the ASME Boiler and Pressure Vessel Code - Section VIII, Div 1 for pressure vessels and Section I for boilers. All of the recommendations for PWHT by P-No and nominal thickness are provided.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources