INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Zinc Oxide - French vs American Process

Zinc Oxide - French vs American Process

Zinc Oxide - French vs American Process

(OP)
Can anyone tell me if there is a difference in performance of American process Zinc Oxide as compared to French process Zinc Oxide in polychloroprene compounds? I want to sub French process zinc oxide for American process zinc oxide due to supply concerns. Formula is general purpose based on a G-type CR. Thanks.

RE: Zinc Oxide - French vs American Process

Should be less concern going that way, as the "French process" generally gives a purer product.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources