B31.3 section K
B31.3 section K
(OP)
If the wps used for production welding requires PWHT is it required to perform PWHT on welder qualifications also? Is mechanical testing of performance tests per ASME IX required for section K?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: B31.3 section K
Yes & Yes
Regards,
DD
RE: B31.3 section K