INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Plate or Forging A48-C1 : Where is it coming from ?

Plate or Forging A48-C1 : Where is it coming from ?

Plate or Forging A48-C1 : Where is it coming from ?

(OP)
Hello all,
I hope someone can help.
a) According to NF A 36-205 (Edition 1982) Plates A 48 exist in three variants AP, CP and FP .
If a certification after heat treatment is necessary, a guarantee can be given and the three variants are followed by an "R"
(ex. A 48 APR, A 48 CPR and A 48 FPR) .
b) The same nuances exist in forgings according to NF A 36-605 (Edition 1982)
c) We are asked to find equivalent to A 48-C1
  As the metal is for a head submitted to pressure, both plate and forging can be suitable.
d) Having a copy of NF A 36-205, I analyzed attentively the document without finding any mention to any C1 variant.
e) I have searched for an answer in the Stahlschlüssel 2013 Edition (German Key to Steels) without success .
f) I suspect the C1 variant to be imposed by another French Regulation (CODAP, ...)
   After an analysis in CODAP Part 1 - 2000 Edition - Paragraph "Base Metals" Table MA6.1 I can find the reference  of NF A 36-205 + NF A 36-605  // A48FP (Plate and Forging): Nothing about variant C1 .
Can someone explain where base metal A 48-C1 is coming from and what does C1 variant imply as additional requirement ?
Sincerely,
A_Tsampalas
 

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources