INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

13% Cr material

13% Cr material

13% Cr material

(OP)
Good day,

We have placed an order to vendor for the supply of Gas Lift Mandrel (Material grade L-80 13%Cr) as per API 19G1 standard and shall meet sub-class E1 (for stringent environmental condition like sour service H2S etc)" As per this standard mandrls shall be monogrammed as API 19G1 "E1".
Now vendor has come up with issue that 13%Cr material cannot be used for sour service application and hence, cannot be monogrammed to sub class E1.

My questions are:

1) Can we use 13%Cr material for sour service application ?? As far as I know as per API 5CT, L80-13%Cr material can be used for sour service application subject to satisfactory passing of SSC test as per NACE TM-0177. Please advise....

2) If not, then vendor could have proposed other material grade which can be used for sour service application during tendering stage?? Please correct me if I am wrong ......

Regards


RE: 13% Cr material

Review 6.3.2 of API Spec 19G1 and Table A.19 of ISO 15156-3. Of the five environmental parameters that apply in Table A.19, how many did you provide to the manufacturer such that they could classify the material?

Steve Jones
Corrosion Management Consultant

http://www.linkedin.com/pub/8/83b/b04

All answers are personal opinions only and are in no way connected with any employer.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources