I am interested in TEEK as an insulation material for a reusable food carrier.
I am interested in TEEK as an insulation material for a reusable food carrier.
(OP)
Polyimide-Foam/Aerogel Composites for Thermal Insulation
I am interested in TEEK as an insulation material for a reusable food carrier.
We are prototyping using Urethane blow molding.
Heat retention is satisfactory but could be improved.
Weight is definitely a problem.
The cost is way too high.
We are looking for solution and found TEEK!
Can TEEK be blow molded? Can it form a skin like Urethane?
Is the cost better compared with Urethane?
I am interested in TEEK as an insulation material for a reusable food carrier.
We are prototyping using Urethane blow molding.
Heat retention is satisfactory but could be improved.
Weight is definitely a problem.
The cost is way too high.
We are looking for solution and found TEEK!
Can TEEK be blow molded? Can it form a skin like Urethane?
Is the cost better compared with Urethane?





RE: I am interested in TEEK as an insulation material for a reusable food carrier.
TTFN

FAQ731-376: Eng-Tips.com Forum Policies
Need help writing a question or understanding a reply? forum1529: Translation Assistance for Engineers