INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

AWS d1.1 essential variable clarification

AWS d1.1 essential variable clarification

AWS d1.1 essential variable clarification

(OP)
Hi

Can i use a pre-qualified AWS D1.1 WPQ , where the base material is S355 to S355, and now I want to use this qualification to weld S355 to S275 .

IS this allowed in AWS essential variable .

RE: AWS d1.1 essential variable clarification

A prequalified WPS must use a base metal that is listed in Table 3.1. If it isn't listed, it ain't a prequalified WPS.

Best regards - Al

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources