INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Arc

Arc

(OP)
Hello There,

Customers are requesting us make connector housings out of DAP because they are concerned about arc tracking resistance. I wanted to ask if anyone knows of any test data comparing the arc resistance performance of DAP (Diallyl Phthalate) as compared to Fortron (PPS, etc.) Also, are there any new thermoplastics that would be acceptable alternatives to DAP as far as arc tracking performance? Thank you in advance for any information you might provide. Bill B.

P.S.:
From some of my literature, I found the following data:

PPS:
Arc Resistance per ASTM D495 is 34 seconds.
Arc tracking rate per UL746A is 20 inches/min.
Comparative tracking index per UL 746A is 180 volts.

DAP:
Arc resistance ranges from 125 to 190 seconds.


William H. Bernhart, P.E.
 
 
I work as a development engineer for AMP - Tyco Electronics located near Harrisburg, PA. I help design interconnections and electrical connectors for aerospace applications.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources