INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Cryogenic temperatures

Cryogenic temperatures

Cryogenic temperatures

(OP)
What would be the temperature range if it is suppose to be "Cryogenics"?

RE: Cryogenic temperatures

Depends on the industry and application.
In general industrial guys would consider any liquid gas handling as being cryo.
But for specialists they usually are thinking much colder, say 20K or less.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube

RE: Cryogenic temperatures

Typically, a temperature whereby air is liquified would clearly be considered to be cryogenic, i.e., 78 K. But, any temperature where skin and tissue damage can readily occur should be included, such as anything below 200 K, but NIST says anything below 150 K should be considered to be cryogenic http://cryogenics.nist.gov/AboutCryogenics/about%2...

TTFN
FAQ731-376: Eng-Tips.com Forum Policies

Need help writing a question or understanding a reply? forum1529: Translation Assistance for Engineers

RE: Cryogenic temperatures

(OP)
Noticed that Cryogenic temperature lies between −150 °C (−238 °F) to absolute zero (−273 °C or −460 °F)....

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources