PARTIAL JOINT PENETRATION
|
RE: PARTIAL JOINT PENETRATION
You can make use of a Pre-Qualified WPS as per Sec.3 of AWS D1.1 Code provided that your construction code is AWS D1.1 and the welding variables are with in the range specified in the code .
RE: PARTIAL JOINT PENETRATION
As you have posted in the ASME section then yes, you do need a qualified WPS,
Regards,
DD