AWS D17.1 2G on PQR qualify a rolling 2G?
AWS D17.1 2G on PQR qualify a rolling 2G?
(OP)
I am reviewing a welding procedure PQR. It is for a plate welded in 2G position, but the actual part is a bellows circumferential weld to machined components on either end. it is likely to be a rolling 2G instead. Does a 2G qualify a rolling 2G?





RE: AWS D17.1 2G on PQR qualify a rolling 2G?
Thus the answer is yes, the 2G coupon is adequate.
RE: AWS D17.1 2G on PQR qualify a rolling 2G?
"Does a 2G qualify a rolling 2G?"
Did you actually mean "Does a 2G qualify a rolling 1G ?"
Cheers,
DD