ASME 16.5-2013 has no Pressure-Temperature ratings table for A182 Gr. F60 (Duplex SS 2205 Forgings)
ASME 16.5-2013 has no Pressure-Temperature ratings table for A182 Gr. F60 (Duplex SS 2205 Forgings)
(OP)
Hello,
ASME B16.5-2013 has no Pressure-Temperature ratings table for A182 Gr.F60 (Duplex Stainless Steel 2205) forgings. For example Table II 2-2.8 includes working pressure for A182 Grades F44, F51, F53 & F55 but no information for A182 Gr. F60. If i have to use this flange, how i can calculate the working pressure. Also, if i have to order this flange, i can't even specify the ASME code B16.5 in flange description, since this grade is not in ASME B16.5.
Please advise.
Thanks,
Meck91
ASME B16.5-2013 has no Pressure-Temperature ratings table for A182 Gr.F60 (Duplex Stainless Steel 2205) forgings. For example Table II 2-2.8 includes working pressure for A182 Grades F44, F51, F53 & F55 but no information for A182 Gr. F60. If i have to use this flange, how i can calculate the working pressure. Also, if i have to order this flange, i can't even specify the ASME code B16.5 in flange description, since this grade is not in ASME B16.5.
Please advise.
Thanks,
Meck91





RE: ASME 16.5-2013 has no Pressure-Temperature ratings table for A182 Gr. F60 (Duplex SS 2205 Forgings)