Smart questions
Smart answers
Smart people
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Member Login

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips now!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!

Join Eng-Tips
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

LINK TO THIS FORUM!

Add Stickiness To Your Site By Linking To This Professionally Managed Technical Forum.
Just copy and paste the
code below into your site.

Partner With Us!

"Best Of Breed" Forums Add Stickiness To Your Site
Partner Button
(Download This Button Today!)

Feedback

"...this web site is a 'Godsend' for me. If I have a programming problem that I'm unable to solve, I'll get a sensible reply in no time. It's really great!..."

Geography

Where in the world do Eng-Tips members come from?
aspearin1 (Chemical)
8 Nov 02 17:38
Is there a strong affinity for SiO2 (weakly negative) to bind to Primary amines?  Or Quaternary amines? More specifically, on a high amine nylon membrane?  We're having a slight contamination issue, but we're not quite sure if it's an issue yet.
EMKWR (Chemical)
25 Nov 02 7:43
Membranes are known to suffer scaling effects. This could be the deposition of carbonates but in case of high SiO2-contents, silicates will do as well. There is no real connection with the material used for the membrane, the presence of a polyvalent cation (calcium, magnesium for example) will do. Have seen a great picture recently at the UPW Europe of a membrane which has doubled in weight because of the deposition of insoluable salts.
You should try the addition of some anti-scalant.

Edwin Muller
e.f.muller@kema.nl

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!

Close Box

Join Eng-Tips® Today!

Join your peers on the Internet's largest technical engineering professional community.
It's easy to join and it's free.

Here's Why Members Love Eng-Tips Forums:

Register now while it's still free!

Already a member? Close this window and log in.

Join Us             Close