INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Shell insert

Shell insert

Shell insert

(OP)
I am trying to find out if a proposed shell insert plate would be acceptable per code; I will attempt to describe it since I cannot attach a picture:

-The shell insert plate would be 24" x 24" and it would intersect the cornerweld at a 90 degree angle
-The insert will placed along an existing vertical weld and the horizontal weld would intersect this vertical weld at a 90 degree angle
-There will only be one rounded corner

I think that it cannot be installed this way because:
-API 653 section 9.2.2.1 describes the repalcement plate as having "rounded corners", which to me means it needs to have at least 2
-secondly, Figure 9.1 in API 653 does not show this to be an "acceptable" layout and one of the patches shown in this figure crosses the vertical weld by at least V or needs to stay away from a vertical weld by at least V

Your opinions would be greatly appreciated. Thank you.

RE: Shell insert

Sounds acceptable to me. Couple of 'compliance' points;
Weld the vert first, to allow the hoop shrinkage from the weld to occurr unimpeded, then weld the corner.
Ensure that the rounded corner on the insert is generous - 2" min. radius, but more is better. Watch for notches and other 'oopses' where the corner transitions into the flat side - they create stress concentrations.
Finally, weld all of one side of the corner weld and perform the required 'diesel oil' leak test prior to starting on the other side.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources