Alternative to Sulfuric acid
Alternative to Sulfuric acid
(OP)
We manufacture brass casings for the military. One of the steps is to clean the brass after annealling. This is to remove the oxidation that occurs with a sulfuric acid, then wash. Is there an alternative to using the sulfuric acid that isn't as corrosive, without bringing in carcinogins, strong alkali's, etc.?





RE: Alternative to Sulfuric acid
http://www.crewscorp.com/AR-696Tech.pdf
RE: Alternative to Sulfuric acid
RE: Alternative to Sulfuric acid
Matt
Quality, quantity, cost. Pick two.