INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Material Properties standard

Material Properties standard

Material Properties standard

(OP)
Hi,

i wanted to know if there is any EN/European standard for material properties similar to ASME Section 2 Part D (for pressure vessels).

-Mohankumar

RE: Material Properties standard

Short: no.
Theyre scatterd in all the different product form standards like EN 10216, 10088, 10222, etc.

RE: Material Properties standard

(OP)
Thanks...

RE: Material Properties standard

A list of much used European materials and their standards can be found in EN 13445-2 for pressure vessels and EN 13480-2 for piping.

RE: Material Properties standard

(OP)
Thanks OSIRIS7.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources