INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Plian Welded Steel Wire Mesh - Standards

Plian Welded Steel Wire Mesh - Standards

Plian Welded Steel Wire Mesh - Standards

(OP)
Our old master specification for plain (un-deformed) welded steel wire mesh (like 6x6 6/6 etc. ) referenced CSA Standards G30.3 and G30.5. but those standards have been discontinued by CSA quite some time ago (although I understand that they can still be purchased from CSA). CSA at the time they were discontinued, said to replace them with ASTM A82 and A185. But on checking the ASTM web site, it says that these standards are superseded.

Question:

What standard(s) should we specify for plain welded steel wire mesh?

RE: Plian Welded Steel Wire Mesh - Standards

(OP)
sorry for the typo in the header...it should say "plain"

RE: Plian Welded Steel Wire Mesh - Standards

ASTM A1064 replaced the old plain and deformed wire and welded wire specifications.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources