INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Temperatures - ASTM Ranges

Temperatures - ASTM Ranges

Temperatures - ASTM Ranges

(OP)
Hey everyone!

I have read lot of ASTM Standards say, Specification is for High and Intermediate temperature Applications or Specification is for Low and Moderate temperature Application. Is there any ASTM Standard which classify this temperature ranges

Thanks in advance!

RE: Temperatures - ASTM Ranges

No, because the ASTM standard specifications are typically referenced by international design codes and standards which permit use of various materials and further define service temperature applications.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources