INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Section VIII, Div. 1, 2013 HAZ Impacts

Section VIII, Div. 1, 2013 HAZ Impacts

Section VIII, Div. 1, 2013 HAZ Impacts

(OP)
I am trying to determine the number of HAZ impacts to be taken in accordance with the new edition of the Code. I typically qualify plates that are 1.5 inches thick with a partial penetration groove of 3/4 inch. Fig. UG-84.5 seems to specify CJP welds with "t" being the base metal thickness. Since I am welding partial penetration welds, can the weld metal thickness be "t"?

RE: Section VIII, Div. 1, 2013 HAZ Impacts

Yes, the weld thickness is t because beyond this it is all base material and is not affected by welding.

RE: Section VIII, Div. 1, 2013 HAZ Impacts

(OP)
Thanks!

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources