INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Qualification for Liquid Penetrant Testing

Qualification for Liquid Penetrant Testing

Qualification for Liquid Penetrant Testing

(OP)
What level of personnel qualification is required to perform a liquid penetrant test on a Section VIII vessel? Our personnel have completed Level 1 and 2 classes.

RE: Qualification for Liquid Penetrant Testing

Please review UW-54 of ASME Section VIII, Div 1 and Section V (T-150) so that you can fully understand what is required and learn more about the code.

RE: Qualification for Liquid Penetrant Testing

(OP)
Thanks. Those parts of the code are exactly what I was looking for. My concentration is on design,so I don't normally deal with test procedures and qualifications. That's usually handled by the QA Manager, but management has me involved with this for some reason.

RE: Qualification for Liquid Penetrant Testing

Qualification requirements are defined in Mandatory Appendix 8. Qualification need not be per SNT-TC-1A.

RE: Qualification for Liquid Penetrant Testing

[all of the above, plus] the usual scheme is that a Level III writes and approves the testing procedures, and Level II's perform those tests i.a.w. those procedures. L/II can work w/o supervision*, and can be the 'final signature' on a test report. L/I's have to work under direct supervision by a L/II or L/III, and have to have their reports countersigned by a L/II or L/III.

L/III is required to perform random audits of the L/II's and L/I's performing testing, to ensure that they are working within the boundaries of the approved procedure.

RE: Qualification for Liquid Penetrant Testing

(OP)
Thanks, Duwe6. That was pretty much my understanding of the code. Our Level 2 guy was trained and examined by a certified Level 3. Prior to his training, which is recent, we have always outsourced all of our NDT. Our testing procedure policy was therefore the procedure that the vendor used with the vendor doing the testing. We are now looking to develop our own in-house procedure, thus the reason for training one of our own inspectors. Our game plan is to develop a procedure using SNT-TC-1A as a guide and submit that procedure to an AI for approval. We would then have additional personnel certified by a Level 3.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources