INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

QUALIFICATION THICKNESS LIMITS ASME IX

QUALIFICATION THICKNESS LIMITS ASME IX

QUALIFICATION THICKNESS LIMITS ASME IX

(OP)
Hi,

What is de T range if:

SMAW - Plate 15 mm - V-groove - P6 - PWHT and Impact tested in PQR

Table QW-451.1 ASME IX said: Over 3/8 (10), but less than 3/4 (19) = 2T for T for base metal.

Someone told me that T = 1.1 x T because Impact test and PWHT performed during the PQR

Is that so and where is this described in te ASME IX?

Thnx!
Patrick

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources