INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Pre-packaged, Nonshrink Grout Testing

Pre-packaged, Nonshrink Grout Testing

Pre-packaged, Nonshrink Grout Testing

(OP)
We are supporting a project demanding strict quality. The client is proposing to use Non-shrink grout under base-plates and other structural components. We can not find an ASTM Standard that specifically addresses "Field" testing of the grout.

We have referenced the following ASTMs:
C 109
C 942 (manufacturer's recommendation)
C 1107

These touch and go on the subject of field sampling/testing, but very vague. We are in the process of writing a project/task-task specific procedure to encapsulate all requirements, and would appreciate helpful input.

Any suggestions/recommendations?

RE: Pre-packaged, Nonshrink Grout Testing

There is no site sampling for a product like non-shrink grout. The standards for acceptance are laboratory tests. Many masonry mortar/grout standards have requirement on proportions and mixing, but field sampling is not really productive. the only thing to do is make sure the materials are used according to proportioning or pre-proportioned materials are mixed and used as required.

Even the common masonry mortar does not have field tests, but the proportions are determined by lab tests to meet the various types of mortar.

It is a site control requirement to be enforced by the specifier of the product/material.

Dick

Engineer and international traveler interested in construction techniques, problems and proper design.

RE: Pre-packaged, Nonshrink Grout Testing

For grouted PT projects, we site sample 2" cubes (steel moulds) and lab test them for 7-day and 28-day compressive strength.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources