INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Regarding ASME B 31.3 RT acceptance criteria.

Regarding ASME B 31.3 RT acceptance criteria.

Regarding ASME B 31.3 RT acceptance criteria.

(OP)
We have 9.5 mm thickness butt welded joints.

Category:Normal fluid service.

Question: Maximum acceptable size in rounded indication within the cluster porosity.

As per ASME B 31.3 for normal fluid service, rounded indication shall be 1.5 X D.

So,for random rounded indication shall be 1/4t i.e 1/4 X 9.5 mm = 2.31 mm (As per ASME Sec VIII Div.1 App-4, table 4-1). Also written in App-4 maximum permisible size 1/4t or 5/32(4mm) whichever is lesser.

Now my question is, when we go for interpretation of cluster porosity as per B31.3 then what is the maximum size of rounded indication within the cluster porosity?

It is 1.5 X 2.31 = 3.46 mm or 2.31 mm.

Request to explain me.

Regards
Prithvi




Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources