INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Degreasing solvent

Degreasing solvent

Degreasing solvent

(OP)
hello fellas

What is the best vapour degreasing solvent that can replace trichloroethylene? or even if is a strong alkaline degreaser.

This solvent is to remove oil and grease soil.

RE: Degreasing solvent

Identifying the "best" would require knowledge of multiple factors. You can do your own research, here are some to look at:

Vapor degreasing: DuPont Vertrel specialty fluid, various suppliers of n-propyl bromide

Detergent cleaning: numerous products from multiple suppliers, e.g. Henkel Parco Cleaner 800 or Chemetall Gardoclean S 5065 or SurTec 199

RE: Degreasing solvent

I wish people would stop asking for "best" anything. In engineering, "best" is usually not possible, since there are almost always compromises to be made, for cost, for usability, for environmental, etc. Without a detailed constraint space, there is no "best"

TTFN
FAQ731-376: Eng-Tips.com Forum Policies

Need help writing a question or understanding a reply? forum1529: Translation Assistance for Engineers

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources