Hi
my Elliptical Dished head material of contraction is SA 240 GR 316Ti same Grade is not mention in Table UHA-44.
Requirement of post forming Heat treatment for material grade which is not listed Table UHA-44
where I need to refer for this ? any one have official interpretation of ASME ?
regards
mechyp
my Elliptical Dished head material of contraction is SA 240 GR 316Ti same Grade is not mention in Table UHA-44.
Requirement of post forming Heat treatment for material grade which is not listed Table UHA-44
where I need to refer for this ? any one have official interpretation of ASME ?
regards
mechyp





RE: Post Froming Req. as per UHA-44( for material that not listed in table)
RE: Post Froming Req. as per UHA-44( for material that not listed in table)
I know that SS316 post forming strain limit may be considers for its relevant grade such as SS316Ti but how can I convey to my client.
any where in ASME Section VIII DIV-I or II clearly expressed as u mention in your reply or any interpretation for that.
thanks
mechyp
RE: Post Froming Req. as per UHA-44( for material that not listed in table)
RE: Post Froming Req. as per UHA-44( for material that not listed in table)
In which clause of Section VIII, Div 1. that code case was incorporated?
mechyp
RE: Post Froming Req. as per UHA-44( for material that not listed in table)
RE: Post Froming Req. as per UHA-44( for material that not listed in table)
RE: Post Froming Req. as per UHA-44( for material that not listed in table)
RE: Post Froming Req. as per UHA-44( for material that not listed in table)
thanks for reply metengr