INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

CHS TO CHS WELDED CONNECTIONS ACCORDING TO AWS

CHS TO CHS WELDED CONNECTIONS ACCORDING TO AWS

CHS TO CHS WELDED CONNECTIONS ACCORDING TO AWS

(OP)
i have a chs to chs welded connection, the required weld is a cjp weld, after checking the AWS 2010 i found details for the welding procedure described in figures 3.6 , 3.7 3.8 , 3.9 3.10

my question is can anyone tell me gow can i determine the area for each detail!!

i mean for example the heel area has its own details , but how can i determine the heel area in the connections!!

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources