INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Minimum cover for Class V RCP

Minimum cover for Class V RCP

Minimum cover for Class V RCP

(OP)
Hi,

What is the recommended minimum cover over Class V RCP? Where can it be found? Any help much appreciated.

RE: Minimum cover for Class V RCP

Cover requirements for RCP depend on the applied loading, quality of the bedding and, of course, the class of pipe. The American Concrete Pipe Association has prepared tables for highway loading. Here is the link to "LRFD Fill Height Table for Concrete Pipe":
http://www.concrete-pipe.org/pdf/FillHeightTables....

Note that Class V pipe that you are asking about is suitable for highway loading with only 1 foot of cover (the minimum shown in the tables) even if there is no bedding at all (Type 4 Installation). One foot is generally considered minimum cover for practical purposes. You did not state the loading for your application, but if it is higher than highway loading, you may need either more cover or a "Special Design" pipe.

www.SlideRuleEra.net idea
www.VacuumTubeEra.net r2d2

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources