Chemical Composition
Chemical Composition
(OP)
What section in the ASME Code would I find the Chemical Composition requirments for 5454 Aluminum?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: Chemical Composition
RE: Chemical Composition
RE: Chemical Composition
Alloy Silicon Iron Copper Manganese Magnesium Chromium Zinc Titanium Aluminum
5454 0.25 0.40 0.10 0.50–1.0 2.4–3.0 0.05–0.20 0.25 0.20 remainder