Geometry Factors
Geometry Factors
(OP)
Can anyone recommend a good resource(s) for obtaining elastic and plastic geometry factors in regards to Linear Elastic Fracture Mechanics (LEFM) and Elastic Plastic Fracture Mechanics (EPFM) respectively?
thanks,
thanks,





RE: Geometry Factors
Paris and Tada
haven't seen plastic geometry corrections ?
Quando Omni Flunkus Moritati
RE: Geometry Factors
Stress Intensity Factors Handbook
Murakami, 1987
Handbook of Stress Intensity Factors
Sih, 1973