INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

API 5L X52 pipe bend Test

API 5L X52 pipe bend Test

API 5L X52 pipe bend Test

(OP)
HI Everyone
i have just joined this forum
i am in urgent need for some info
i need to do 1 Root Bend & 1 Face bend for API 5L X52 Pipe
diameter of pipe is 350 and wall thickness is 12.7mm
Can anyone please advise me the Mandrel diameter i have to use for bends and what is the test method for bend test for API pipe
Thanks

RE: API 5L X52 pipe bend Test

Obtain a copy of API 1104. It is available online for a price, but if you are qualifying the WPS or the welder, you need it.

Best regards - Al

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources