INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Application of Self-Locking Patch

Application of Self-Locking Patch

Application of Self-Locking Patch

(OP)
I have a threaded joint that I would like to make self locking. Neither the male or female portion of the joint is a standard fastener, meaning I can't just go out and buy a self locking fastener. I don't want to use an anaerobic locking compound. I have considered drilling the male threads and installing a nylon pellet per Mil-Dtl-18240 Type N. But I wondered if anyone sells a product that cold be used to create your own spray on patch. I've been searching the internet but have only seen the finished product - screws with a patch already on them. In my case, I want to buy the patch material, and spray it on in the shop.

Has anyone done this that could point me in the right direction?

Thanks!

RE: Application of Self-Locking Patch

(OP)
Thanks MintJulep. I had looked at this site before. I don't think they sell a product to make patches. I believe they will apply the patch for you or sell you a fastener with the patch already applied. The user applied products are compounds similar to Loctite products. What I am looking for is a user applied patch.

RE: Application of Self-Locking Patch

I think the VC-3, VC-4, VC-5 or VC-6 products do what you are asking.

They are paint on, rather than spray.

RE: Application of Self-Locking Patch

Lots of brake and suspension hardware comes with some gunk pre-applied.
http://www.fcpeuro.com/products/volvo-brake-calipe...

They are considered one time use, at least by the manufacturer.
I'm guessing they are treated with a product similar to those found by MintJulep

RE: Application of Self-Locking Patch

(OP)
Thanks for all the help. It looks like the ND Industries products were closer to what I was looking for than what I thought. I appreciate the input.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources