Material Spec. for All Thread Rod with Tensile between 90-110ksi?
Material Spec. for All Thread Rod with Tensile between 90-110ksi?
(OP)
I need to find all thread rod with a tensile strength between 90-110 ksi. I've contacted a few steel houses and can't seem to find anything in their inventory. Is there a material spec. that is around grade 70 with a UTS of 90-110 ksi? The rod sizes are 1/2".
Thanks,
M
Thanks,
M





RE: Material Spec. for All Thread Rod with Tensile between 90-110ksi?
RE: Material Spec. for All Thread Rod with Tensile between 90-110ksi?
RE: Material Spec. for All Thread Rod with Tensile between 90-110ksi?
1/2" all thread rod is widely available in ASTM A193 gr.B7 (125ksi UTS/105ksi YTS) or gr.B7M (100ksi UTS/80ksi YTS).