INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Metal Qustion

Metal Qustion

Metal Qustion

(OP)
Have Prints of 1929 Willys Night Sleeve valve Engine .
Can not Cross Cylinder Iron M-11 To Modern Gray Iron or Similer .
Operation of engine is Valve less type , 2 sliding sleeves with piston in middle of inner sleeve .Intake Ports on left side of engine and exahust ports on Right Side . Both Sleeves are in The Combustion Chamber .
Sleeves were Normalized at 900 Degres for One Hour and Slowly Cooled For 7 hours .
Most notacable Relation is Malleable Iron . But also has Grey Iron charactoristics . Any help would Be Appreciated

RE: Metal Qustion

High graphite content grey iron is what you want for a cylinder liner. Your heat treat sounds correct.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources