INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

A36 mod plate with CE 0.3 to 0.33

A36 mod plate with CE 0.3 to 0.33

A36 mod plate with CE 0.3 to 0.33

(OP)
Hi,
I'm new at this forum.
I just have a quick question that someone here might be able to help me.
I have a client that is requesting some A36 Mod plate to have a CE value between 0.3 min to 0.33 max and I'm having no luck finding. I wanted to ask if this plate is something that might be common or if I will have a difficult time finding. The majority of the plate I'm needing is 3/16" thk to 3/4" x 96" x 240". I have ran into a few but they have all been 1/4" x 120" x 240". If anyone can guide me or at least tell me this is nearly impossible, I would really appreciate any advise.

Thanks,
CadChick
Houston, TX

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources