What was the alloy mentioned in this post? thread330-240321: Spring wire material for use in high pressure hydrogen gas?
http://www.sei.co.jp/tr_e/pdf/industrial/61-09.pdf
http://www.sei.co.jp/tr_e/pdf/industrial/61-09.pdf





RE: Alloy name; link no longer active.
a search in google scholar gives:
http://global-sei.com/tr/pdf/industrial/61-09.pdf
TTFN

FAQ731-376: Eng-Tips.com Forum Policies
Need help writing a question or understanding a reply? forum1529: Translation Assistance for Engineers
RE: Alloy name; link no longer active.
It is an austenitic stainless steel that does not transform to martensite during wire drawing or spring coiling. Click on the link and you can download the paper (.pdf) for free.